Economical: 10% masterbatch at .35 plus 90% rPET at .40 gives you a total raw material cost of .75 cents per pound.
Processing: Dry Nylester masterbatch at 185 F for 2 hours until moisture is .005%. Then add 10% masterbatch to rPET chips to the extruder used to make pellets. Product is now called Nylester6
Packageing: 25-50 Lb. samples are available! Production =1000 lbs
Cost: $3.50 per pound fob Dalton Ga. (10% let down = .35Cents.
ASTM Test Standards Enginering Nylon 6
www. aquadyefibers.com
Heat Deflection or Melt Temp. 250C, Tensil Strength 8000 + = Nylon 6,
Flexural Modulus 349 = Nylon 6 Izod Impact .359 = Nylon 6
Nylester masterbatch innovation expands the end-use applications of PET or rPET in molded or extruded products. Use in place of Engineering Nylon6!